Re: [PSUBS-MAILIST] Hot Dip Galvanizing a Steel Sub Hull



You don't, huh? Ever see a rust spot on a chrome or nickel job on a motorcycle?
Vance


-----Original Message-----
From: Brian Cox <ojaivalleybeefarm@dslextreme.com>
To: personal_submersibles@psubs.org
Sent: Tue, 2 Jun 2009 12:37 pm
Subject: RE: [PSUBS-MAILIST] Hot Dip Galvanizing a Steel Sub Hull

Frank,
       Nickel plating is frequently used in a saltwater environment.  I don't see how you could get a pin hole in a 1/4" or 3/8" hatch, the plating is going to ADD material to the existing steel.
 
Brian
-----Original Message-----
From: owner-personal_submersibles@psubs.org [mailto:owner-personal_submersibles@psubs.org]On Behalf Of ShellyDalg@aol.com
Sent: Tuesday, June 02, 2009 8:38 AM
To: personal_submersibles@psubs.org
Subject: Re: [PSUBS-MAILIST] Hot Dip Galvanizing a Steel Sub Hull

How ya been Brian? Ya, nickel plating would look good, almost like chrome! Might look into that.
I think nickel plating would still need a protective coating for salt water operations.
Anybody know of a good clear coat for salt water?
How's your sub doing? Got any new pictures? Let me know the hext time you're up here, lunch is on me. Frank D.