[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

RE: [PSUBS-MAILIST] 40 degree inclusive angle Vee clamps for Viewports




Hey Jay,

Right, I was just thinking that the moly anti-seize would keep the mating parts from being as conductive and keep every thing out, as well as be easy to apply, clean up, and remove the parts.  

Vance did you apply any thing to the SS mating surfaces on the Vee clamping rings and pods for dealing with corrosion?  Did you ever see any corrosion in those areas?

Regards,
Szybowski





From: bottomgun@mindspring.com
To: personal_submersibles@psubs.org
Subject: RE: [PSUBS-MAILIST] 40 degree inclusive angle Vee clamps for Viewports
Date: Sun, 1 Mar 2009 18:12:45 -0500

Brent,

Moly anti-seize is not a bedding compound.  Red lead is but there are many better products out there…red lead is the traditional material.

R/Jay

 

Respectfully,

Jay K. Jeffries

Andros Is., Bahamas

 

As scarce as the truth is, the supply has always been in excess of the demand.

    -Josh Billings

 

 

 

From: owner-personal_submersibles@psubs.org [mailto:owner-personal_submersibles@psubs.org] On Behalf Of Brent Hartwig
Sent: Sunday, March 01, 2009 5:59 PM
To: PSUBSorg
Subject: RE: [PSUBS-MAILIST] 40 degree inclusive angle Vee clamps for Viewports

 



So use the moly grease or the red lead product?


Szybowski