Re: [PSUBS-MAILIST] Hot-galvanize stainless steel ?
That is it - I put the last solution on
http://www.prismnet.com/~moki/subfiles.html
shown as "X2".
I will made the bottom cover plate from zinc..
We have a lot of used old zinc-anodes here on the
yard - I will heat one or two to liquid stage and
make three custom zinc-anodes-cover plates..
They can be easy replace by a diver - just pressuzies
the diverchamber to 0,22 bar - open the bottom hatch
(see at "X13") jump out and replace the three plates
with a screwdriver one times a year - maybe possible
in summer times without a scuba gear..
thank you to everbody.. Carsten
ronleonard schrieb:
>
> What's wrong with just using a sacrificial anode on your drop weight? So
> long as you keep it active, shouldn't that prevent your corrosion
> problem?
> Ron