Hi Brian,
Stanley Plastics charged me £120 (about $200) per 8" viewport made to
PVHO. I didnt think that was too bad for peace of mind.
Kind Regards
James
On 1 April 2014 17:01, Brian Cox <brian at ojaivalleybeefarm.com> wrote:
> Hi Doug,
> I think I'm going to see what finished windows would
> cost me from Hydrospace. The chamber for the annealing would need to be
> completely re-thought out. I was thinking that maybe an enclosed liquid,
> like antifreeze, could be used to circulate through a special chamber that
> would be surrounded with the liquid. That way you could really get a
> handle on the exact temperature of a circulating liquid. But still you have
> to change the temp, maybe a mixing valve. But by the time I got through
> with that I could probably buy a number of viewports !
>
> Attached is a shot of the stresses I induced with my bad annealing attempt
>
> Brian
>
>
>
>
>
>
>
>
> My sympathies Brian. I'm sorry that your experimental annealing didn't
> go well, but as they say, it is always better to try and fail than fail to
> try. It sounds like perhaps you just need to make some modifications to
> your oven to better regulate temperatures, but I'm sure that is easier said
> than done. Are you planning to make another attempt? ~ Douglas S.
>
>
> On Tue, Apr 1, 2014 at 10:49 AM, Brian Cox <brian at ojaivalleybeefarm.com>wrote:
>
> Epic Fail ! my attempt to anneal a viewport did not go well. The
> temps swings were so great that it was impossible to regulate. The mass in
> the oven that I had hoped would moderate the swings made it so the lag time
> between the heating cycle and when the thermometer sensor saw the
> temperature change uncontrollable. And the heat was not even though out
> the oven as well.
>
> Brian
>
> --- hanker_20032000 at yahoo.ca wrote:
>
> From: hank pronk <hanker_20032000 at yahoo.ca>
> To: Personal Submersibles General Discussion <
> personal_submersibles at psubs.org>
> Subject: Re: [PSUBS-MAILIST] annealing acrylic
> Date: Tue, 25 Mar 2014 05:35:51 -0700 (PDT)
>
> Brian,
> I say when in doubt, test. If your not building a test chamber , you can
> make your sample window to fit my chamber and I will test it for you.
> Hank
>
>
> On Monday, March 24, 2014 7:23:18 PM, Brian Cox <
> brian at ojaivalleybeefarm.com> wrote:
> Hank,
> I have the book, that's where the annealing schedules are, they
> vary quite a bit, there is an absolute minimum time and then there is the
> original recommended time. The recommended time comes out to be around 51
> hours where as the shortened time is maybe half that. I'm just doing one
> test piece to start off with. I was also using the same oven ( a toaster
> oven I got from Sears for $75 bucks) to heat the welding rod to 250 degrees
> F before we used the rod ( it had been sitting out for a few days). I was
> able to keep the temperature fairly even for the welding rod at 250.
>
> Brian
>
> --- hanker_20032000 at yahoo.ca wrote:
>
> From: hank pronk <hanker_20032000 at yahoo.ca>
> To: Personal Submersibles General Discussion <
> personal_submersibles at psubs.org>
> Subject: Re: [PSUBS-MAILIST] annealing acrylic
> Date: Mon, 24 Mar 2014 17:39:27 -0700 (PDT)
>
> Brian,
> Do you have the Stachiw book of Acrylics, I can send you mine if you don't
> have a copy. There is some pretty important stuff in there.
> Hank
>
>
> On , hank pronk <hanker_20032000 at yahoo.ca> wrote:
> Brian,
> How thick is your acrylic? should take more than a night?
> Hank
>
>
> On Monday, March 24, 2014 6:33:09 PM, Brian Cox <
> brian at ojaivalleybeefarm.com> wrote:
> Yes, I have the annealing schedules. I have an electric oven and two
> digital thermometers, one I'm going to put in a piece of acrylic and the
> other one I'm going to use to monitor the oven temperature itself . I'm
> worried that the thermometer in the acrylic won't register until it gets
> heated throughout, and so then the oven temp might go higher than it
> should. So between the two readouts I can heat it gradually up. It'll be
> a long night.
>
> Brian
>
> --- hanker_20032000 at yahoo.ca wrote:
>
> From: hank pronk <hanker_20032000 at yahoo.ca>
> To: Personal Submersibles General Discussion <
> personal_submersibles at psubs.org>
> Subject: Re: [PSUBS-MAILIST] annealing acrylic
> Date: Mon, 24 Mar 2014 17:22:32 -0700 (PDT)
>
> Brian,
> Are you going to anneal your windows yourself?
> Hank
>
>
> On Monday, March 24, 2014 6:03:10 PM, Brian Cox <
> brian at ojaivalleybeefarm.com> wrote:
> Used my polarized lenses on the newly cut piece and it appears clouded
> throughout the whole piece. Where as another piece I have, you can clearly
> see a stress area around where it has been drilled.
>
> Brian
>
>
> --- emile at airesearch.nl wrote:
>
> From: "Emile van Essen" <emile at airesearch.nl>
> To: "'Personal Submersibles General Discussion'" <
> personal_submersibles at psubs.org>
> Subject: Re: [PSUBS-MAILIST] annealing acrylic
> Date: Mon, 24 Mar 2014 22:40:46 +0100
>
> As far as I know it is only cast.
>
> Regards, Emile
>
> *Van:* Personal_Submersibles [mailto:
> personal_submersibles-bounces at psubs.org] *Namens *Brian Cox
> *Verzonden:* maandag 24 maart 2014 20:37
> *Aan:* PSubs
> *Onderwerp:* [PSUBS-MAILIST] annealing acrylic
>
> I'm planning on annealing my viewports, does anyone know if the acrylic
> from the factory is pre-shrunk ?
>
> Brian _______________________________________________
> Personal_Submersibles mailing list Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
> _______________________________________________
> Personal_Submersibles mailing list
> Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
>
> _______________________________________________ Personal_Submersibles
> mailing list Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
> _______________________________________________
> Personal_Submersibles mailing list
> Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
>
>
>
> _______________________________________________ Personal_Submersibles
> mailing list Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
> _______________________________________________
> Personal_Submersibles mailing list
> Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
>
> _______________________________________________ Personal_Submersibles
> mailing list Personal_Submersibles at psubs.org<http://eonapps/ft/wm/page/compose?send_to=Personal_Submersibles%40psubs.org>
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
> _______________________________________________
> Personal_Submersibles mailing list
> Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
>
> _______________________________________________ Personal_Submersibles
> mailing list Personal_Submersibles at psubs.org<http://eonapps/ft/wm/page/compose?send_to=Personal_Submersibles%40psubs.org>
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
> _______________________________________________
> Personal_Submersibles mailing list
> Personal_Submersibles at psubs.org
> http://www.psubs.org/mailman/listinfo.cgi/personal_submersibles
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://www.whoweb.com/pipermail/personal_submersibles/attachments/20140401/7b6e257c/attachment.html>
More information about the Personal_Submersibles
mailing list